Abstract
Ultrahigh-strength steels are designed to be used in structural applications where very high loads are applied and often high strength-to-weight ratios are required. This article discusses the composition, mechanical properties, processing, product forms, and applications of commercial structural steels capable of a minimum yield strength of 1380 MPa (200 ksi). These include medium-carbon low-alloy steels, such as 4340, 300M, D-6a and D-6ac steels; medium-alloy air-hardening steels, such as HI1 modified steel and H13 steel; high fracture toughness steels, such as HP-9-4-30, AF1410, and AerMet 100 steels; and maraging steels.
Sign in
ASM members
Member Sign InUltrahigh-Strength Steels, Metals Handbook Desk Edition, 2nd Ed., 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 260–265, https://doi.org/10.31399/asm.hb.mhde2.a0003101
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.