Abstract

Cast stainless steels are widely used for their corrosion resistance in aqueous media at or near room temperature and for service in hot gases and liquids at elevated temperatures. This article provides a comparison between cast and wrought stainless steels in terms of composition, microstructure and properties. It discusses the grade designations and compositions of cast stainless steels. The article describes the mechanical properties, applications, and corrosion characteristics of corrosion-resistant steel castings and heat-resistant steel castings.