Abstract

This article provides an overview of the classification system of coppers for conductors and for wires and cables, as well as wire rod fabrication techniques such as rolling and continuous casting. Wiredrawing and wire stranding operations, including the preparation of rod surface, drawing, production of flat rectangular wire, annealing, and coating, are discussed. The article also provides information on electrical insulation and jacketing techniques, including polymeric insulation, enamel insulation, and paper-and-oil insulation.