Aluminum and its alloys are used in a broad range of applications. This article discusses the primary and secondary production of aluminum and the classification system for cast and wrought products. It describes some of the more common manufactured forms, including commercial wrought aluminum products, aluminum alloy engineered castings, powder metallurgy parts, and metal-matrix composites. The article also reviews fabrication characteristics such as machining, forming, forging, and joining. It concludes with a description of the major industrial applications of wrought and cast aluminum alloys.

Abstract

This article describes the systems for designating the aluminum and aluminum alloys that incorporate the product forms (wrought, casting or foundry ingots) and its respective temper for strain-hardened alloys, heat-treatable alloys and annealed alloys. All these systems are covered by American National Standards Institute (ANSI) standard H35.1. Furthermore, the article provides a short note on the designation of unregistered tempers.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal