Abstract
Chemical elements are the basic chemical substances; that is, they cannot be decomposed by chemical change or made by chemical union. These elements follow a periodic pattern related to the atomic mass of each that allows them to be arranged into a convenient table. This article includes a series of tables: the first gives the names and symbols of the elements in alphabetical order and the second lists the elements in order by atomic number and give the atomic weight for each. The periodic table of the elements also is included in the article.
Abstract
Crystal structure is the arrangement of atoms or molecules in the solid state that involves consideration of defects, or abnormalities, in idealized atomic/molecular arrangements. The three-dimensional aggregation of unit cells in the crystal forms a space lattice or Bravais lattice. This article provides a brief review of the terms and basic concepts associated with crystal structures. It also discusses some of the significant defects obstructing plastic flow in real crystals, namely point defects, line defects, stacking faults, twins, and cold work. Several tables in the article provide information on the crystal structures and lattice parameters of allotropes of metallic elements.
Sign in
ASM members
Member Sign InStructure and Properties of Metals, Metals Handbook Desk Edition, 2nd Ed., 2nd ed., Edited By Joseph R. Davis, ASM International, 1998
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.