Wet lay-up using hand or spray techniques is one of the simplest methods of combining a fiber reinforcement with a solidifying resin to form a composite structure. This article describes several wet lay-up processes - including contact molding, spray molding, vacuum bag molding, and autoclave molding - suited for making parts on open-faced molds using polyester and vinyl ester resins. The article also provides information on mechanically assisted lay-up which can be automated to alleviate some of the manual work.

You do not currently have access to this chapter.
Don't already have an account? Register

1995. "Hand Lay-Up, Spray-Up, and Mechanical Lay-Up", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier