Sheet molding compound (SMC) is a composite material - consisting of glass-fiber-reinforced polyester in a resin matrix - that’s available in sheet form for the production of compression-molded parts. This article discusses the components incorporated into the resin paste, including catalysts, fillers, thickeners, pigments, thermoplastic polymers, flame retardants, and ultraviolet absorbers, and how to optimize them to achieve the desired processing and molding characteristics and the necessary properties in the resulting parts. The article also presents several mixing techniques, including batch, batch/continuous, and continuous mixing, and describes the operations of continuous-belt and beltless machine type SMCs.

You do not currently have access to this chapter.
Don't already have an account? Register

1995. "Sheet Molding Compounds", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal