Rotational molding is a simple but unique process that has the capability of producing small to large hollow items with very uniform wall thicknesses. Providing an overview of the operating principles of rotational molding, this article discusses the key selection factors, including function and property requirements for resins and additives; size, shape, design, and cost of molded parts; equipment type and size; and the type of mold to be used. Commonly used molds include cast aluminum, fabricated sheet metal, nickel deposit, machined aluminum, silicone, fiberglass, and prototype molds.