Abstract

This article describes the chemical composition, physical properties, thermal properties, mechanical properties, electrical properties, optical properties, magnetic properties, and chemical properties of glasses, glass-matrix composites, and glass-ceramics.

You do not currently have access to this chapter.
Don't already have an account? Register

Design and Engineering Properties of Glasses, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 1171–1187, https://doi.org/10.31399/asm.hb.emde.a0003066