This article reviews the fundamental relationships between microstructure and mechanical properties for major classes of nonmetallic engineering materials: metals, ceramics and glasses, intermetallic compounds, polymers, and composites. It details the structures of inorganic crystalline solids, inorganic noncrystalline solids, and polymers. The article describes the various strengthening mechanisms of crystalline solids, namely, work hardening, solid-solution hardening, particle/precipitation hardening, and grain size hardening. Deformation and strengthening of composite materials, polymers, and glasses are reviewed. The article concludes with information on the two important aspects of the mechanical behavior of any class of engineering material: fatigue response and fracture resistance.

You do not currently have access to this chapter.
Don't already have an account? Register

M.L. Weaver, M.E. Stevenson, 2000. "Introduction to the Mechanical Behavior of Nonmetallic Materials", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal