This article is a comprehensive collection of tables that list the values for hardness of plastics, rubber, elastomers, and metals. The tables also list the tensile yield strength and tensile modulus of metals and plastics at room temperature. A comparison of various engineering materials, on the basis of tensile strength, is also provided.

Abstract

This article is a compilation of terms related to mechanical testing and evaluation of metals, plastics, ceramics, and composites.