Abstract
This article reviews the general mechanical properties and test methods commonly used for ceramics and three categories of polymers, namely, fibers, plastics, and elastomers. The mechanical test methods for determining the tensile strength, yield strength, yield point, and elongation of plastics include the short-term tensile test, the compressive strength test, the flexural strength test, and the heat deflection temperature test. The most commonly used tests for impact performance of plastics are the Izod notched-beam test, the Charpy notched-beam test, and the dart penetration test. Two basic test methods for a group or strand of fibers are the single-filament tension and tow tensile tests. Room temperature strength tests, high-temperature strength tests, and proof tests are used for testing the properties of ceramics.
Sign in
ASM members
Member Sign InMechanical Testing of Polymers and Ceramics, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 26–48, https://doi.org/10.31399/asm.hb.v08.a0003256
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.