ASM Handbook
Mechanical Testing and Evaluation
Edited by
ASM International
Volume
8
ISBN electronic:
978-1-62708-176-4
Publication date:
2000
Abstract
This article describes methods that are oriented toward the analysis of planned cooperative experiments that involve multiple factors, blocks, and/or treatment levels. The experiments include factorial, fractional factorial, randomized block, and incomplete block experiments.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Analysis of Designed Experiments, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, https://doi.org/10.31399/asm.hb.v08.a0009215
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.