Abstract

This article provides a discussion on the equipment used and specimen preparation for microindentation hardness testing (MHT) such as the Vickers hardness test and the Knoop hardness test. It describes the important test considerations to be considered during MHT. The article also discusses the most common hardness conversions and the applications of MHT.