High Strain Rate Shear Testing
-
Published:2000
Abstract
This article reviews the dynamic factors, experimental methods and setup, and result analysis of different types of high strain rate shear tests. These include high strain rate torsion testing, double-notch shear testing and punch loading, drop-weight compression shear testing, thick-walled cylinder testing, and pressure-shear plate impact testing.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
High Strain Rate Shear Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 447–461, https://doi.org/10.31399/asm.hb.v08.a0003295
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.