This article describes the fatigue mechanism and behavior of environmentally induced fatigue and cyclic fatigue. It discusses three basic strength test methods, namely, static, dynamic, and cyclic, along with their analytical relations for determining the fatigue parameters and behavior of ceramics and glasses. The article explains the double torsion and double-cantilever beam fracture mechanics methods, which employ test specimens with relatively large, induced cracks. Crack growth data are typically determined directly by the observation of the crack or by devices that monitor test specimen compliance, such as clip gages and strain gages.

You do not currently have access to this chapter.
Don't already have an account? Register

J.A. Salem, M.G. Jenkins, Fatigue Testing of Brittle Solids, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 768–778, https://doi.org/10.31399/asm.hb.v08.a0003319

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal