Abstract

This article reviews the fundamentals of electrochemical corrosion test methods. The features and requirements of the instrumentation needed for an electrochemical test are briefly discussed. The article provides a discussion on the various electrochemical techniques and tests available for laboratory studies of corrosion phenomena. The techniques and tests include no-applied-signal tests, small-signal polarization tests, large-signal polarization tests, scanning electrode techniques, and miscellaneous techniques.

You do not currently have access to this chapter.
Don't already have an account? Register

Florian Mansfeld, 2003. "Electrochemical Methods of Corrosion Testing", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.