This article discusses factors that influence the effect of alloying, metallurgical treatments, and mechanical treatments on the corrosion resistance of metallic materials, with schematic illustrations.

You do not currently have access to this chapter.
Don't already have an account? Register

Paul Natishan, 2003. "Introduction to Corrosion Resistance of Bulk Materials", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.