This article provides an introduction on the metal side of the corrosion reaction and describes a wide range of metallurgical factors that influence corrosion.

You do not currently have access to this chapter.
Don't already have an account? Register

G.S. Frankel, 2003. "Introduction to Metallurgically Influenced Corrosion", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.