This article addresses electrochemical methods for instantaneous rate determination and threshold determination as well as nonelectrochemical methods that can determine incremental or cumulative rates of corrosion. Electrochemical methods for the study of galvanic corrosion rates and localized corrosion and evaluation of corrosion rates under paints are also discussed. The article describes nonelectrochemical methods that can determine incremental or cumulative rates of corrosion. Methods presented include polarization methods, polarization resistance methods, electrochemical impedance methods, frequency modulation methods, electrochemical noise resistance, potential probe methods, cyclic potentiodynamic polarization methods, potentiostatic and galvanostatic methods, electrochemical noise (EN) methods, scratch-repassivation method, and electrochemical impedance spectroscopy (EIS) techniques. Gravimetric determination of mass loss, electrical-resistance methods, magnetic methods, quartz crystal microbalance method, solution analysis methods, and metrological methods are nonelectrochemical methods. The article presents an electrochemical test that examines the susceptibility of stainless steel alloys to intergranular corrosion.

You do not currently have access to this chapter.
Don't already have an account? Register

John R. Scully, Robert G. Kelly, 2003. "Methods for Determining Aqueous Corrosion Reaction Rates", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal