When planning a corrosion-testing program, it is advisable to select the testing conditions carefully in order to produce ranking parameters with minimal influence from testing conditions while rich in engineering significance. This article provides a discussion on test objectives, metal composition and metallurgical conditions, test specimen preparation, and corrosion damage assessment. It describes a strategy for planning the design of controlled and uncontrolled factorial experiments. The article contains a table that lists the elements of an iterative process for the experimental design. It illustrates the experimental designs applied to corrosion testing.

You do not currently have access to this chapter.
Don't already have an account? Register

P.R. Roberge, 2003. "Designing, Planning, and Preparing Corrosion Tests", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal