This article begins with a discussion on the classification of hydrogen embrittlement and likely sources of hydrogen and stress. The article describes several hydrogen embrittlement test methods, including cantilever beam tests, wedge-opening load tests, contoured double-cantilever beam tests, rising step-load tests, and slow strain rate tensile tests. It also describes the interpretation of test results and how to control hydrogen embrittlement during production.

You do not currently have access to this chapter.
Don't already have an account? Register

Bopinder Phull, 2003. "Evaluating Hydrogen Embrittlement", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.