This article describes the criteria for selecting a corrosion-monitoring method used in industrial plants. It provides a detailed discussion on the design, advantages, and disadvantages of plant corrosion-testing program. The basic types of racks used to support and insulate the coupons are also discussed. The analysis of electrical-resistance probes, sentry holes, side-stream loop, electrochemical noise, hydrogen-probe, and process streams are used to monitor and estimate corrosion rates. The corrosion rates can also be estimated by ultrasonic thickness measurements, polarization-resistance measurements, corrosion potential measurements, and alternating current impedance measurements. Corrosion monitoring strategies, such as locations, data analysis, redundancy, and other issues, are discussed. The article concludes with information on the interpretation and reporting of corrosion testing.

You do not currently have access to this chapter.
Don't already have an account? Register

Sheldon W. Dean, 2003. "Corrosion Monitoring for Industrial Processes", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal