Abstract

This article provides a discussion on the operation of various methods and sensors that have been used or have the potential to be used for on-line, real-time monitoring of localized corrosion. These include the electrochemical noise (ECN) method, nonelectrochemical methods, the galvanically coupled differential flow cell, galvanically coupled crevice cell, coupled multielectrode sensor, and electrochemical biofilm activity sensor.

You do not currently have access to this chapter.
Don't already have an account? Register

Lietai Yang, Narasi Sridhar, 2003. "Monitoring of Localized Corrosion", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.