This article presents common conventions and definitions in corrosion, electrochemical cells, cathodic protection (CP), electricity, and oxidation. Evans diagrams for impressed current CP in neutral or basic environment and galvanic or sacrificial CP, in both neutral or basic environment and acidic environment, are illustrated.