Simulated service testing includes exposures of either structural components or test specimens in environments that are representative of many general service situations. This article discusses the selection criteria of test specimens and methods of assessing the corrosion effects. The ASTM International and NACE International standards that are directly or indirectly applicable to simulated service corrosion testing in water are tabulated. The article also describes the effects of variable concentrations of dissolved carbonates, such as calcium, magnesium, and/or sodium, in water on corrosion.