Abstract
This article discusses the factors affecting corrosion behavior. It describes galvanic corrosion and its protection methods. The article also provides information on coatings and inhibitors, which are used in corrosion protection.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Paul Natishan, Introduction to Methods of Corrosion Protection, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 685–686, https://doi.org/10.31399/asm.hb.v13a.a0003672
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Corrosion of Wrought Stainless Steels
Corrosion: Materials
Corrosion of Magnesium and Magnesium-Base Alloys
Corrosion: Materials
Corrosion of Zinc and Zinc Alloys
Corrosion: Materials
Corrosion of Organic Coated Steels
Corrosion: Materials
Pickling and Descaling
Surface Engineering
Corrosion of Hafnium and Hafnium Alloys
Corrosion: Materials
Corrosion of Aluminum and Aluminum Alloys
Corrosion: Materials
Corrosion of Zirconium and Zirconium Alloys
Corrosion: Materials
Magnesium Alloys
Lightweight Materials Understanding the Basics
Beryllium
Lightweight Materials Understanding the Basics