Abstract

Molten salts, or fused salts, can cause corrosion by the solution of constituents of the container material, selective attack, pitting, electrochemical reactions, mass transport due to thermal gradients, and reaction of constituents and impurities of the molten salt with the container material. This article describes a test method performed using thermal convection loop for corrosion studies of molten salts. It discusses the purification of salts that are used in the Oak Ridge molten salt reactor experiment. The article also reviews the corrosion characteristics of nitrates/nitrites and fluoride salts with the aid of illustrations and equations.