Abstract

The corrosion process that occurs in industrial systems is often difficult to discern until extensive deterioration has occurred. For boilers to function properly, the incoming water must be processed to meet the water quality required for the boiler. This article discusses pretreatment methods of the incoming water and preboiler corrosion protection methods. It analyzes internal treatment and condensate treatment of boilers. The article discusses three types of cooling systems: once-through systems, open recirculating systems, and closed recirculating systems. The corrosion processes which occur in water-recirculating systems and the effect of dissolved gases, temperature, pH, suspended solids, dissolved salts, and scale deposition on corrosivity of water, are also reviewed. The article also considers anodic and cathodic inhibitors and the control of corrosion in municipal water systems.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal