Abstract

Crevice corrosion is a form of localized corrosion that affects many alloys that normally exhibit passive behavior. This article discusses the frequently used crevice corrosion testing and evaluation procedures. These procedures include specific crevice corrosion tests, multiple-crevice assembly tests, cylindrical materials and products evaluation, component testing, electrochemical tests, and mathematical modeling.