Inorganic chemical-setting ceramic linings are one of the most widely used construction materials in designing the protective linings for industrial installations. Monolithic linings can be applied by cast or gunite (shotcreting) methods over steel or concrete as well as brick and mortar masonry. This article provides a discussion on the function of monolithic linings, the advantages of these materials, the types of applications in which these materials can be successfully used, and the limitations of these linings. It describes the application procedures that should be followed to ensure proper installation of a dual-lining system. The industrial applications that illustrate the corrosion resistance and some uses of monolithic linings, as well as other applications in wastewater treatment systems and the chemical industry, are discussed.

You do not currently have access to this chapter.
Don't already have an account? Register

Chemical-Setting Ceramic Linings, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 755–758, https://doi.org/10.31399/asm.hb.v13a.a0003684

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal