Skip to Main Content
Skip Nav Destination

Abstract

This article provides a discussion on the fundamentals of corrosion thermodynamics. The discussion focuses on electrochemical reactions, molten salt corrosion thermodynamics, and geochemical modeling.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal