Abstract

The two major types of beryllium-containing alloys are copper-berylliums and nickel-berylliums. The most widely used beryllium-containing alloys are wrought copper-berylliums, which provide good strength while retaining useful levels of electrical and thermal conductivity. This article provides information on the specimen preparation procedures, macroexamination, microexamination, and microstructures of beryllium, copper-beryllium alloys, as well as nickel-beryllium alloys. It also discusses health and safety measures associated with the specimen preparation of beryllium and beryllium-containing alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

John C. Harkness, Amitava Guha, 2004. "Metallography and Microstructures of Beryllium, Copper-Beryllium, and Nickel-Beryllium Alloys", Metallography and Microstructures, George F. Vander Voort

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal