This article describes the microcrack analysis of composite materials using bright-field illumination, polarized light, dyes, dark-field illumination, and epi-fluorescence.

You do not currently have access to this chapter.
Don't already have an account? Register

Brian S. Hayes, Luther M. Gammon, 2004. "Microcrack Analysis of Composite Materials", Metallography and Microstructures, George F. Vander Voort