This article describes the various aspects relating to the selection and preparation of ultrathin-section specimens of fiber-reinforced polymeric composites for examination by transmitted light microscopy. It provides information on the contrast-enhancement methods used by transmitted-light microscopy and optimization of microscope conditions. Examples of composite ultrathin sections analyzed using transmitted-light microscopy contrast methods are also presented.

You do not currently have access to this chapter.
Don't already have an account? Register

Brian S. Hayes, Luther M. Gammon, 2004. "Thin Section Preparation and Transmitted Light Microscopy for Fiber-Reinforced Composites", Metallography and Microstructures, George F. Vander Voort