Pure metals normally solidify into polycrystalline masses, but it is relatively easy to produce single crystals by directional solidification from the melt. This article illustrates the dislocations present in a metal crystal, which is often polygonized into sub-boundaries during grain growth after solidification. It provides a description of small-angle and large-angle grain boundaries of polycrystalline metals.