Microstructural analysis reveals many important details about the qualities and capabilities of high-performance ceramics. This article explains how to prepare ceramic samples for imaging and the imaging technologies normally used. It describes sectioning, mounting, grinding, and polishing as well as ceramographic etching. It discusses common imaging approaches, including scanning electron microscopy and thin-section polarized light techniques, a type of optical microscopy. The article also addresses microstructural classification, examining detailed micrographs from samples of aluminum oxide, zirconium dioxide, aluminum nitride, silicon carbide, and piezoelectric ceramics.

You do not currently have access to this chapter.
Don't already have an account? Register

Ulrike Täffner, Veronika Carle, Ute Schäfer, Michael J. Hoffmann, 2004. "Preparation and Microstructural Analysis of High-Performance Ceramics", Metallography and Microstructures, George F. Vander Voort

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal