Grit Sizes and Grain Size Conversions
-
Published:2004
Publication history
November 01, 2004
Abstract
This article contains a conversion table, which assists in the conversion of ASTM number to average grain intercept length. It also includes a table that lists European and U.S. grit numbers with their approximate particle size for metallographic grinding papers.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Grit Sizes and Grain Size Conversions, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 1093, https://doi.org/10.31399/asm.hb.v09.a0003726
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Measurement of Microstructure
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Superplastic Deformation at Elevated Temperatures
Mechanical Testing and Evaluation
Metallography and Microstructures of Copper and Its Alloys
Metallography and Microstructures
Metallography and Microstructures of Zinc and Its Alloys
Metallography and Microstructures
Liquid Metal Induced Embrittlement
Corrosion: Fundamentals, Testing, and Protection
Effect of Crack Shape on Fatigue Crack Growth
Fatigue and Fracture
Multiaxial Fatigue Strength
Fatigue and Fracture
Mechanisms of Corrosion Fatigue
Fatigue and Fracture
Fatigue and Fracture of Nickel-Base Superalloys
Fatigue and Fracture
Heat Treating of Uranium and Uranium Alloys
Heat Treating of Nonferrous Alloys