Abstract
This article discusses the metallography and microstructures of carburized, carbonitrided, and nitrided steels, with illustrations. It provides information on the widely used metallographic techniques including sectioning, mounting, grinding and polishing, and etching.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Metallography and Microstructures of Case-Hardening Steel, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 627–643, https://doi.org/10.31399/asm.hb.v09.a0003762
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Metallography and Microstructures of Lead and Its Alloys
Metallography and Microstructures
Metallography and Microstructures of Zinc and Its Alloys
Metallography and Microstructures
Metallography and Microstructures of Zirconium, Hafnium, and Their Alloys
Metallography and Microstructures
Metallography and Microstructures of Tin and Tin Alloys
Metallography and Microstructures
Metallography and Microstructures of Carbon and Low-Alloy Steels
Metallography and Microstructures
Metallography and Microstructures of Heat-Resistant Alloys
Metallography and Microstructures
Metallography and Microstructures of Low-Carbon and Coated Steels
Metallography and Microstructures
Metallography
Inspection of Metals Understanding the Basics
Preparation and Microstructural Analysis of High-Performance Ceramics
Metallography and Microstructures
Metallography and Microstructures of Refractory Metals and Alloys
Metallography and Microstructures