Abstract
Lightning damage in polymer composites is manifested by damage at both the macroscopic or visual level and within the material microstructure. This article illustrates the effects of the laboratory-generated lightning strikes on polymeric composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Brian S. Hayes, Luther M. Gammon, Analysis of the Effects of Lightning Strikes on Polymeric Composites, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, https://doi.org/10.31399/asm.hb.v09.a0009085
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Pipeline Failure Results from Lightning Strike: Act of Mother Nature?
Handbook of Case Histories in Failure Analysis
Visual Examination and Light Microscopy
Fractography
Use of Fractography for Failure Analysis
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Metallographic Technique for Nonferrous Metals and Special-Purpose Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Eutectic Alloy Systems
Phase Diagrams Understanding the Basics
Peritectic Alloy Systems
Phase Diagrams Understanding the Basics
Forging of Nickel-Base Alloys
Metalworking: Bulk Forming
Workability in Forging
Metalworking: Bulk Forming
Bulk Forming of Intermetallic Alloys
Metalworking: Bulk Forming
Models for Predicting Microstructural Evolution
Metalworking: Bulk Forming