Metallography and Microstructures
Abstract
Mounting of the specimen is often desirable or necessary for handling and metallographic polishing after the specimen is cut into an appropriate size. This article illustrates the different mechanical clamps used in mounting small specimens. It provides useful information on compression molded mounts, which are molded with thermoplastic and thermosetting resins. The article reviews several resins and their key factors, which help in the selection of the most appropriate mounting method and resin. It also discusses the characteristics of plastic mounting materials. The article provides information on the molds and resins used for castable mounts, vacuum treatment of mounts, special mount arrangements, and mount marking and storage.
Sign in
ASM members
Member Sign InMounting of Specimens, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 242–256, https://doi.org/10.31399/asm.hb.v09.a0003786
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.