Metallography and Microstructures
Field Metallography Techniques
-
Published:2004
Abstract
This article discusses the advantages and disadvantages of field metallography and describes the important material characteristics and other aspects to be considered before performing any metallographic procedure. It investigates the various stages of sample preparation in the metallographic laboratory: grinding, polishing, etching, preparing a replica, and obtaining a small sample. The article also illustrates the applications of field metallography with case studies.
Sign in
ASM members
Member Sign InBruce L. Bramfitt, Samuel J. Lawrence, Field Metallography Techniques, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 478–492, https://doi.org/10.31399/asm.hb.v09.a0003751
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.