Metallography and Microstructures
Thin Section Preparation and Transmitted Light Microscopy for Fiber-Reinforced Composites[1]
-
Published:2004
Abstract
This article describes the various aspects relating to the selection and preparation of ultrathin-section specimens of fiber-reinforced polymeric composites for examination by transmitted light microscopy. It provides information on the contrast-enhancement methods used by transmitted-light microscopy and optimization of microscope conditions. Examples of composite ultrathin sections analyzed using transmitted-light microscopy contrast methods are also presented.
Sign in
ASM members
Member Sign InBrian S. Hayes, Luther M. Gammon, Thin Section Preparation and Transmitted Light Microscopy for Fiber-Reinforced Composites, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, https://doi.org/10.31399/asm.hb.v09.a0009076
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.