Abstract
This article contains tables that list standard reduction potentials for electrochemical reactions. The first table lists reactions alphabetically by element of interest. The second table is ranked by potential value. Potential is measured versus the Standard Hydrogen Electrode which has a value of 0.0000 V. Reactions with more than one voltage indicate that results have not been reconciled. Parenthetical materials not needed to balance reactions are catalysts.