Spinodal Transformation Structures
By
-
Published:2004
Publication history
November 01, 2004
Abstract
Spinodal transformation is a phase-separation reaction that occurs from kinetic behavior. This article discusses the theory of spinodal decomposition, and outlines the methods used in the characterization of spinodal structures in metal matrices.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Shane Para, Spinodal Transformation Structures, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 140–143, https://doi.org/10.31399/asm.hb.v09.a0003732
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Intermediate Phases
Alloy Phase Diagrams
Eutectic Alloy Systems
Phase Diagrams Understanding the Basics
Peritectic Alloy Systems
Phase Diagrams Understanding the Basics
Forging of Nickel-Base Alloys
Metalworking: Bulk Forming
Workability in Forging
Metalworking: Bulk Forming
Bulk Forming of Intermetallic Alloys
Metalworking: Bulk Forming
Models for Predicting Microstructural Evolution
Metalworking: Bulk Forming
Forging of Heat-Resistant Alloys
Metalworking: Bulk Forming
Plastic Deformation Structures
Metalworking: Bulk Forming
Recovery, Recrystallization, and Grain-Growth Structures
Metalworking: Bulk Forming