Metallography and Microstructures
Metallography and Microstructures of Nickel and Nickel-Copper Alloys
-
Published:2004
Abstract
This article explains how to prepare nickel-base alloys for metallographic examination and identifies related processing and imaging challenges. It describes sectioning, mounting, grinding, and polishing procedures along with alternative electropolishing processes. It also provides information on etching and examines the microstructure of Nickel 200, Nickel 270, Duranickel 301, Monel 400, Monel R-405, Monel K-500, and other nickel alloys.
Sign in
ASM members
Member Sign InWilliam L. Mankins, Metallography and Microstructures of Nickel and Nickel-Copper Alloys, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 816–819, https://doi.org/10.31399/asm.hb.v09.a0003775
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.