Introduction to Transformation Structures
By
Arnold R. Marder
Arnold R. Marder
Department of Materials Science and Engineering, Lehigh University
Search for other works by this author on:
-
Published:2004
Publication history
November 01, 2004
Abstract
This introductory article provides basic information on the various aspects of solid-state transformation: multiphase microstructures, substructures, and crystallography, which assist in characterizing the morphology of phase transformations. It contains a flowchart that illustrating the classification of transformations by growth processes.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Arnold R. Marder, Introduction to Transformation Structures, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 132–133, https://doi.org/10.31399/asm.hb.v09.a0003730
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Synchrotron X-Ray Diffraction Applications
Materials Characterization (2019 Edition)
Low-Energy Electron Diffraction
Materials Characterization (2019 Edition)
Cobalt and Cobalt Alloy Castings
Casting
Modeling and Simulation of Texture Evolution during the Thermomechanical Processing of Titanium Alloys
Fundamentals of Modeling for Metals Processing