Metallography and Microstructures of Lead and Its Alloys
-
Published:2004
Publication history
November 01, 2004
Abstract
This article describes the various specimen preparation procedures for lead, lead alloys, and sleeve bearings, including sectioning, mounting, grinding, polishing, and etching. The microscopic examination and microstructures of lead and lead alloys are discussed. The article also provides information on the microstructures of sleeve bearing materials.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Metallography and Microstructures of Lead and Its Alloys, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 789–800, https://doi.org/10.31399/asm.hb.v09.a0003773
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Metallographic Technique for Nonferrous Metals and Special-Purpose Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Metallography
Inspection of Metals Understanding the Basics
Metallographic Practices Generally Applicable to All Metals
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Metallographic Technique for Ferrous Metals
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Lead and Lead Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Heat Treating of Low-Melting-Point Alloys
Heat Treating of Nonferrous Alloys
Thermal Conductivity of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Use of Fractography for Failure Analysis
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Surface Engineering of Nickel and Nickel Alloys
Surface Engineering
Finishing Methods Using Multipoint or Random Cutting Edges
Surface Engineering