Abstract
This article describes the various specimen preparation procedures for lead, lead alloys, and sleeve bearings, including sectioning, mounting, grinding, polishing, and etching. The microscopic examination and microstructures of lead and lead alloys are discussed. The article also provides information on the microstructures of sleeve bearing materials.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Metallography and Microstructures of Lead and Its Alloys, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 789–800, https://doi.org/10.31399/asm.hb.v09.a0003773
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Metallography and Microstructures of Zinc and Its Alloys
Metallography and Microstructures
Metallography and Microstructures of Zirconium, Hafnium, and Their Alloys
Metallography and Microstructures
Metallography and Microstructures of Tin and Tin Alloys
Metallography and Microstructures
Metallography and Microstructures of Case-Hardening Steel
Metallography and Microstructures
Metallography and Microstructures of Carbon and Low-Alloy Steels
Metallography and Microstructures
Metallography and Microstructures of Heat-Resistant Alloys
Metallography and Microstructures
Metallography and Microstructures of Low-Carbon and Coated Steels
Metallography and Microstructures
Metallographic Technique for Nonferrous Metals and Special-Purpose Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Metallography
Inspection of Metals Understanding the Basics
Preparation and Microstructural Analysis of High-Performance Ceramics
Metallography and Microstructures