Abstract

This article describes the metallographic specimen preparation procedures for cast iron test samples, including mounting, grinding, polishing, and etching. It discusses the makeup and use of black-and-white and selective color etchants and where one might be preferred over the other. The article provides information on nearly 100 micrographs, discussing the microstructure of flake graphite in gray iron, nodular graphite in ductile iron, and temper graphite in malleable iron. It also examines the matrix microstructures of gray, ductile, compacted, and malleable cast iron samples.

You do not currently have access to this chapter.
Don't already have an account? Register

Janina M. Radzikowska, Metallography and Microstructures of Cast Iron, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 565–587, https://doi.org/10.31399/asm.hb.v09.a0003765

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal